Lightweight Aggregate - an overview | ScienceDirect Topics
Lightweight aggregates have been produced with pelletisation and thermal treatment of SSA. A limited amount of testing has been undertaken to examine the leaching behaviour of the resultant products. Aggregate pellets, 250 mm in size, produced after sintering at 1050°C, have been assessed using the EPA TCLP (Bhatty et al., 1992).